Default Re: Moisture Problems???

Quote:
Originally Posted by baz View Post
a filter or a separator has to be mounted away from the compressor but not a dryer
when you said a dryer, i was thinking of a refrigirated dryer. what you have there looks more like a dessicant dryer or some other type of filter
then it should be mounted as far as possible from. the compressor

sorry for giving you the wrong info,
also if it is a dessicant unit the dessicant cartrige has to be replaced or dried