Re: My Caswell gun Mods
Thanks for the info. What if I'm not getting any air out of the fluidizer? I'm thinking the fluidizer brings air into the cup pressurizing the cup in turn blowing the powder around (fluidizing/making it lighter) then the vacuum tube picks it up like a mist and disperses it through the tube.
|