Quote:
Originally Posted by afterglow
What tool should I get for a car restoration project?? Stuff to polish include stainless trim and hubcaps, chrome handles, emblems, bezels, etc.
Bench grinder? Die grinder? Electric angle grinder??
|
Bench machine. Beware polishing plated items by machine - you can easily go through the plating.