I'm using the EN process but thought this tidbit might be appropriate.
On the last use of my supposedly "Titanium" tank heater, it plated out in nickel. I never had the problem before (About a year of use) and it came with the kit I purchased. Either it's not titanium or had a thin coating that burned off. I'm not sure which but I thought Ti wouldn't plate in the nickel baths. This stuff did. Just some info to add to your decision.