Im gonna have to email Rosey's about this to see what they think. I roughed up the spots where carb cleaner got, cleaned and degreased the entire part, re-powdered the chrome all over, then put their 100% gloss over on top. Not only did this TURN the chrome powder into an aluminum color (NO reflectiveness at all), but I can still take carb cleaner to it and the powder starts to get sticky and discolor!!!