Default Re: Carb cleaner stripped off chrome powder!!!

Chrome powders require a clear and will turn a silverish/gray. Thats just the nature of the beast. There are single stage chromes but personally I would clear those also. As far as the carb cleaner goes I've heard of people using it to strip powder, why are you putting carb cleaner on it?