Re: help for a new polishing addict
I also do not start sanding with paper that rough. I generally start with 120 also. And like its been said sand 90° to the previous step, so "show" your scratches.
I have not had that good of luck with vintalated flaps. I use spirial wheels for everything.
Yup a wheel for each step, and clean the wheel every once and a wile.
I don't use tripoli, i go from Emory to White.
Good luck, i hope that you can get the results that you desire.
|