I havnt been cleaning the surface after each step.... and I have beed using diff. buffs for eash compound..... I need to get a rake, been cleaning it with a screwdriver...... It makes since to start with 120 or 180 but some of those ford parts are sand cast and have a pitted surface to start...... Im going to spring for a bench buffer but for now Im using a drill
Thanks for the help Ill have a go at it again using the tips