Quote:
Originally Posted by gudgean View Post
try trans black over mirror red.a couple years ago i did my shadow like that.came out great.had darker spots where the black was a little heavy. actually looked like it changed color in the sun.
gudgean is correct. If you use candy red over black, you'll get a maroon red color.