Default Re: help for a new polishing addict

yep and to give you some advice, order the buffs from caswell. i tried the walmart/lowes buffs and compounds and they aren't even close to how well the ones sold here work.

another piece of advice on the blower, remove the compressor housing and do it seperately. it won't have a seal or anything on it, and will come off by just removing those allen key bolts. may need to work it off a bit, but it comes off easily.

that'll also give you a chance to see what kind of wear is on the surface around the compressor wheel