Thread: Few Questions
View Single Post
  #2 (permalink)  
Old 04-09-2008, 02:34 PM
osmondmark osmondmark is offline
Newbie
 
Join Date: Feb 2008
Posts: 28
osmondmark is on a distinguished road
Default Re: Few Questions

I reblasted the parts and cleaned them extremely well! I sprayed them fairly thick but still they are really dull. I need to figure out whats going on and why! I have more parts I need to get started on and got to get these finished!

Do anyone have any suggestions?

BTW Its columbia coatings Super Mirror Orange. Do I need a base coat or anything? I am just spraying it on bare metal.

Here is a pic with the flash off:


Here is one with the flash on:




There is no trouble to see what I am talking about! Thanks for the help!