Quote:
Originally Posted by osmondmark
1) I have done a lot of single stage colors and they all turned out well! Except for the orange tonight but thats another question. I now have a bunch of parts! that I need to do in a candy color. (Blue and gold) Wondering if you have any tips on doing this as it will be my first time doing a candy...
2) Wondering if a metallic blue would require a base coat or clear coat?
3) I sprayed a high gloss orange tonight and it turned out bad! It had like yellow blotches in it and one part was a really really dull yellow. Not bright at all! Just wondering if this could be because of contamination? I am going to blast all the parts again, clean them extremely well, clean the gun spotless and try it again! Any suggestions here?
Thanks a million!
Mark
|
1) Candy colors look best over a polished material or chrome. If applying over something else you need a base coat of something like x-treme chrome.
2) Is the metallic blue a translucent/candy powder? If it is you don't need a clear. If is isn't, I would clear it.
3) I can't see the pics