I ordered the super mirror orange from columbia coatings. I use the super mirror black from them and like it so I figured I would use this. Not sure if they mixed up the powders when packaging or not but I doubt that is the problem, however it could be. Is there anyway to check?
I am going to try the orange again tomorrow for the third time. I am going to blast the hubs and recoat and I am going to just sand the a arms and recoat. I am going to make sure that the coating is thick enough and will try to get as even coverage as possible!
If you have any suggestions you can let me know.
Thanks a million!
|