Quote:
Originally Posted by samtgallagher
so you put compound on your cartridges? any specific types?
|
Baz might use buffing compound if he's found it works, but normally you'd use a high-speed grinder's grease (available here at Caswell). It really is amazing how much smoother the rolls cut with grease, and I've found they cut faster and last longer as well, and it helps keep some of the dust down as well.