A rinse tank is a good way to combat what a spray doesnt get off. Industrial places use something called a cascade rinse system to wash their parts off. Which is a double sided tank, water enters one side from the bottom, flows upward, and overflows into the other side then to the wastewater system. All the chemicals wash upward and over into the other tank, completely washing the parts.