mpierich, can you post the link of the grease that you are talking about. Witch type do you recomend?
Thanks!!!
Look here: http://www.caswellplating.com/buffs/compound2.html

Use the F-10 for high-speed stuff like cartridge rolls; use the F-26 for slower sanding belts, etc. DO NOT use the F-10 for slow speeds...it'll put a glaze on the abrasive that ruins it and is tough to get off even with a belt cleaner.