Re: Finished my oven--some pics too
I fabricated my own sliding hooks out of angle iron and 1/4" round stock. The Unistrut is normally used as a support hanger so I'm not aware of any pre-made sliders/hooks.
If you have a welder the hook/sliders are fairly easy to make. I can post some pictures of the ones I made later today.
|