Re: HD Rocker Box covers coating??
Hot flocked means to shoot the part when it is hot or warm to get good coverage. Normal powder will work fine on these covers.The high temp powders are tempermental and if you screw up your first coat you have to strip and start over again. I have learned the hard way that silcone powders are a one coat deal.
|