Originally Posted by dmend View Post
Here are side and end pictures. The ridges are pretty fine.
Thanks,
dmend
this looks like spinned aluminium ,if it s not too pitted it should be easy to buff .
a tripoli with a spiral sewn or an airflex buff followed by a color compound should get it done