hey, just one more question. Is it possible that the turquoise dye has in some way gone bad and is partially what is causing these marks?
I have two pairs of these same eye covers that I'm doing (one pink, one turquoise) and the pink ones came out fine on my very first try whereas these turquoise ones are still giving me problems. I've been doing them in the same run using the same exact procedure and still the turquoise ones give me "acid dragout-like" blemishes.
|