Question Re: HD Rocker Box covers coating??

Quote:
Originally Posted by powdersparky View Post
Hot flocked means to shoot the part when it is hot or warm to get good coverage. Normal powder will work fine on these covers.The high temp powders are tempermental and if you screw up your first coat you have to strip and start over again. I have learned the hard way that silcone powders are a one coat deal.
I thought regular powders wouldn't be a high enough temp for these. I was told they would burn off because of the temperature the rocker boxes get? I am asking you guys because I trust your opinions and input.