Default Re: Getting better, but not quite right????

Quote:
Originally Posted by Popeye View Post
Could be silicone causing the fish eyes.... waxes and sprays with silicone ruin parts
Popeye,
Find it hard, but not impossible to believe its silicone or wax. I cleaned the part twice with Acetone and once with purple power, which is an industrial strength cleaner/degreaser. Is there something better for cleaning/degreasing available on the market that I can purchase locally??