Anybody had any experience with any POR-15 products? I'm considering the Glisten PC clear for polished aluminum. Does it work or is there something else just a good or better?
|
JAP_NDN,
just came across your post about POR-15. I tried some last winter on my polished front forks and other various motorcycle parts. spent days and days polishing and then applied the POR-15. Was not happy at all with the finished product. i contacted the company and they told me to thin it with Xylene, so I removed all the old POR-15, which took hours and then thinned the POR and did it all over again. SAME results!##%$%^ Threw the S**t away. Save your money.