I've been shooting alot of super mirror black lately and I love the stuff! Always lays out nice and smooth with great coverage. Yet, I'm still having to really heat up the parts to around 230-250. The results are awesome, even with other colors, but I don't think this is common practice...is it?
Anyways, here are a couple pictures of a Nissan valve cover and after market intake manifold that I just finished in super mirror black.