we used 20ga (i think) galvanized steel on 25ga studs. 1/8" aluminum rivets spaced ~6" apart. i used an 1/8" drill bit, so no relief. this is a rather small oven (5x2x1ft), but it's been great. no warping, no noise during heating/cooling.