Default Re: cabinet converted to oven??

Now that you mention it, there must be something in the bottom, because I dont think it would be that heavy just from the steel. But, I'm sure the doors, walls, and top are hollow because they do flex and feel hollow. Also the site I found it listed on per model number, says something to the effect that "all cabinets have an inner wall and an outer wall, to allow for a 1-1/2" air gap."

Also, the inside has a little bit of rust and I was interested in sanding all that off and whenever I get it all wired up- preheat the oven to operating temp, and then opening it up and spraying a good layer of high-temp powder on the whole interior, then closing the doors for the curing time. after the 15 min or whatever I would just turn it off and open the doors to allow it to cool. Will this work?