I have done a lot with coating over it but there is one problem. when it gets hot the stuff bubbles a little bit causeing little bumps all over the place. Some of the powders I use doesn't show them but others do. Also I like to get it off and have the aluminum somewhat shiney so that when I laser engrave on it the back ground is shiney.