Just any color as long as it's bright? I haven't gotten a chance to use very many of caswell's dyes yet, but of those that I have used, fluorescent pink done in gloss is by far the brightest.

Although, I've been told that truly fluorescent colors are a pigment-only thing and can't be achieved with dye.