Angry craters, craters and more more !

Ok iIve about had it with this PC. I've done everything:
1. sanded the T-6061 Aluminum
2. Let it soak in degreaser (purple Power)
3. Washed off and air dried
4. wiped down with Acetone
5. Used torch over piece.
6. wiped again with Acetone
7. torch
8. PC
9. preheated oven to 400 deg.
10. Baked at 392 deg +- 25 degs for 10 minutes

AND STILL I HAVE CRATERS

Someone tell me what more I can do?