Default Re: craters, craters and more more !

Quote:
Originally Posted by holeshot87 View Post
did u outgas it
holeshot87,

I was told i didn't need to outgas as its billet t-6061 aluminum. I did outgas on one coating and the same results.

thanks for your help.

Ben