Green olive drab ph will not rise?? why??
My ph on my olive drab is at 1.6, after talking to guys at Caswell i was told to ad no.2 witch is formic acid to it gradually to increase ph level to 2.2 to 2.7
witch is the best ph level, started with 1/4 bottle nothing happened then 1/2 bottle went to 1.8 then i added whole bottle and it only 1.9, whats going on?? searching for answers, please help, yes im using distilled water, exactly 2 gallons.
|