Re: candy over chrome?
Well I put the super black first cured about 70% and let cool then done the extreme chrome, and then let cool to room temp. Getting ready to apply the clear on a valve cover to try the clear out. I had a brake lever off a atv that I'm trying the lollipop blue on. I didn't seem to have a problem with the chrome covering the part BUT the lollipop blue didn't seem to want to stay on. It was like the powder was trying to blow off. I know that I wasn't too close to the part. It was blowing off near the hanger where I had my ground clip. Is this normal? I think I may have put on too much powder trying to get it to stick because so far the part looks more like a purple than a blue.
|