Default can an ano'ed surface pit?

hello,

can ano'ed layers pit after they are finished under everyday conditions?

there is a debate about what the finish is on another forum in on (finish on macbook pro's) and while they are supposedly "anodized" there has been rare reports of pitting on the palm rests and the finish chipping off. i had a small piece scrape off after it got discolored on and old powerbook with the same finish. i have never seen anodizing react like this at all, nonetheless have the same finish as these computers.

any thoughts/info would be appreciated
-matt