Anodizing doesnt chip under normal conditions. Ive anodized parts and had a small 1/4" spot chip off fresh out of the sealer like a piece of hair thin paint, it has only happened once and I cant explain why. Anodizing shouldn't flake off randomly though. Possibly the metal is plated?