Default Color Variations with the same powder

Hi guys. I'm doing some parts in Candy Blue and some of the parts im doing are turning out a totally different color. I shot 3 pulleys at the same time today. 1 turned out the normal color, 1 was the weird color, and 1 was a mix of the 2.

Is there any way that moisture could be causing this?
So far I tried changing the cure temps up and down - didn't work
I tried applying it thiner and thicker - didn't work

You can see the alternator fan has the right color in the center, but almost everywhere else is the odd color.

I'll try to post some pix
Thanks,
Frank
Attached Thumbnails
color-variations-same-powder-dsc03266-small-.jpg.JPG
Views:	92
Size:	87.1 KB
ID:	1093  color-variations-same-powder-dsc03269-small-.jpg.JPG
Views:	60
Size:	94.8 KB
ID:	1094  

Last edited by LS1Nova; 04-25-2008 at 05:08 PM.
Reply With Quote