Sure is Michael,

The Caswell chrome is hard to get here in Aus due to hazardous freight. Makes it expensive. I'd personally leave the larger chrome bits to a restoration shop, there are heaps around, but definately do the copper/nickel/zinc smaller stuff. I do a lot of restoration on car parts. Everything from brackets and nuts and bolts to pot metal badges and door handles. Chrome plating at a restorers is not that expensive if the part given to them is straight and clean.

Feel free to contact me for any other info.