View Single Post
  #4 (permalink)  
Old 04-27-2008, 04:33 AM
KCV6's Avatar
KCV6 KCV6 is offline
Moderator
 
Join Date: Apr 2007
Location: Adelaide, Australia
Posts: 246
KCV6 is on a distinguished road
Default Re: do the caswell re-charge kits contain wetters

Add wetter... makes a huuuuuuuuuge difference. get a sample of any nickel solution in a small container and shake... if it gets a head of froth that disipates real quick you should add wetting agent. The plate comes out much smoother, like chalk and cheese. wetting agent also helps eliminate hydrogen bubbles forming on horizontal edges.

Still curious to know if the Caswell baths contain wetting agents or not? Someone do the shake test perhaps?