v6 Thanks so much for your help!! learning alot!!Green drab, still has me d.ead in the water, i even called caswell and talked to them, again , i was told to gradually ad formic clear acid to the solution until ph comes up?? I stared by adding 1/4 bottle then 1/2 then the hole bottle, only went from 1.6 recalabrated meter to 1.9 with whole bottle installed, In precisely 2 gals. of distilled water. I love the Caswell products but they really need to get some help with this product. Flat out does not work at all.