Re: Curing... slowly, very slowly
I think you're right. After spending my weekend moving the lamp around, I'm a bit wiser. However, some parts like my Jag cage in the rear end, aren't going to fit in the oven. I'll have to bite the bullet and use the lamp.
I did get the front crossmember and two spring housings done, and the results are satisfactory.
|