View Single Post
  #7 (permalink)  
Old 04-28-2008, 10:24 AM
Travst Travst is offline
Newbie
 
Join Date: Dec 2007
Posts: 26
Travst is on a distinguished road
Default Re: Curing... slowly, very slowly

Thanks for the input. I'm glad I came here to post when I recognized I had a problem. Does anyone have an idea for properly curing the large parts that won't fit into an oven? I'm looking into buildkng a reflector.

Update... found an oven on craigslist for $50... onward, through the fog.

Last edited by Travst; 04-28-2008 at 11:01 AM. Reason: added information