Old 10-23-2003, 07:35 AM
non-stick non-stick is offline
Experienced Metal Finisher
 
Join Date: Sep 2003
Location: CT-NY-NJ area
Posts: 359
non-stick
Default

I don't know about the vinyl mask, but believe it or not.... I've always used electrical tape when I've needed to perform this function. Easily laid down enough and you can trim it with a razor blade to whatever design you wish (through putting a stencil letter on top available at your loacal art store or office supply store or a general "happy face" shape freehand if you will). I lay a patch of tape down and cut out what I need to cut out. Then I re-inforce the lettering or design by putting another layer on top of what I just did on top of where the tape exists still. Works quite well for surface modification for a single piece. Of course....if you need to go into production with more than just the one, I'm sure there's something out there along the lines of what you are thinking. Good luck with it,bud......Russ