I'm not sure what a wetting agent is? I have copy chrome that foams with aeration on, and seems to foam worse when the pH starts to get high.

I've added small amounts of brightener, which usually seems to speed up the need to add muriatic acid to lower the pH... which in turn requires a little hydrogen peroxide to eliminate the rough plate.