View Single Post
  #7 (permalink)  
Old 05-05-2008, 12:12 AM
KCV6's Avatar
KCV6 KCV6 is offline
Moderator
 
Join Date: Apr 2007
Location: Adelaide, Australia
Posts: 245
KCV6 is on a distinguished road
Default Re: best method for heating Zincate solution

Just finished 10 pieces (starter motor end caps, thermostat housings, oil filter adaptors etc). worked MOSTLY fine. These were severely coroded so I ended out with minor blistering on 2 pieces after much copper building, sanding, building, sanding, buil......... where the pits were quite deep. Not enough prep on my part. I'm going to re-work the pitted areas and try a quick re-zincate and see how it goes. Other than that the zincate worked fine.

Cheers

Mark
Reply With Quote