lower the heat and go for a longer cure cycle, back off on the gun and let the "fine" particles attract themselves instead of the bigger ones and see how you do with it then. Remember everybody, this powder is not a substitute for chrome, but a good facade on a surface that "counter-reflects" itself (intake manifold,hood hinges,bracketry,etc) and not a big flat panel. I'm afraid shiny silver that can *almost* be a reflective surface is pretty close to the best you can do with it. In my experience anyways.....Hope that helps, Russ
|