Default Candy help/problem

Hello, I had a slight problem...I used xtream chrome and lolli red on a auto part, xtream chrome went on great, when I put on the lolli red I put it on to thick...While curing some ran down the part or was to thick and is darker/thicker in a small secton..can a sand a small part off? and put on a little bit of red on top? suggestions...I post a pic in a bit. bad part is part looks great and this is the part that is the top...