So a few months ago as I was browsing ColumbiaCoatings I noticed one of the customers examples. which was a gold vein base with a Candy Red on top.
So I ordered some Gold Vein and felt like experimenting on my Honda ecu. I must say Im VERY HAPPY.
Heres the example.
http://store.columbiacoatings.com/pr...6024_image.jpg
Heres mine.