Default Re: Technique for this?

Quote:
Originally Posted by Maicojames View Post
Some parts are just porous all the way through-the more you cut,the more pores you will see, they are not the same pores, but they are there.

So, be wary of any British MC hubs from the 80s and back. JMO.
MJ
Yep. And not to mention most other older parts from many makes as well as some newer ones.