Thanks for the info. Does the aluminum oxide come in different grit sizes? If so, which size for best all around use? I read about black oxide. Is this better or is it all black? We have a Harbor Freight about an hour from here... I know about the sand issue as I read it once on a bag of play sand when I was going to blast some parts with an open air blaster. I prefer to be safe.