yeah, go with one of the caswell starter guns. they'll pay for themselves many times over and you'll learn a lot while saving up for a semi-pro or pro system.

caswell has aluminum oxide in different grits. go with 60 or 80. if you're compressor/blast cabinet is a little low on power, maybe try the 60 first?