Maicojames,

I think the trick here is to not polish through the top layer of the aluminum. If it doesn't have a coating on it (anodized/powder) or a lot of scratches then try using some tripoli on sewn buff. After you cut the top layer off you will get into "pits" thats something you don't want to get into!